A nickel-base superalloy consisting of, by weight: 14.6% to 15.9% cobalt; 11.5% to 13.0% chromium; 0.8% to 1.2% iron; 0.2% to 0.60% manganese; 2.00% to 2.40% molybdenum; 3.30% to 3.70% tungsten; 2.90% to 3.30% aluminum; 2.60% to 3.10% titanium; 3.50% to 5.10% tantalum; 1.20% to 1.80% niobium; 0.10% to 0.60% silicon; 0.02% to 0.06% carbon; 0.010% to 0.030% boron; 0.05% to 0.11% zirconium; up to 0.045% hafnium; and the balance being nickel and impurities.