Polypropylene composition comprising a heterophasic propylene copolymer and a mineral filler, wherein said heterophasic propylene copolymer has a melting temperature in the range of 140 to 155° C., a xylene cold soluble content in the range of 20 to 35 wt.-% and a comonomer content of the xylene cold soluble fraction in the range of 18 to 95 wt.-%, wherein further the weight ratio between heterophasic propylene copolymer and the mineral filler is in the range of 2/1 to 4/1.