Patent attributes
The present invention is directed to a pneumatic tire having a tread comprising a vulcanizable rubber composition comprising, based on 100 parts by weight of elastomer (phr),(A) from about 60 to about 100 phr of a solution polymerized styrene-butadiene rubber having more than 98 percent of the repeat units derived from styrene in blocks containing less than five repeat units, Tg ranging from −65° C. to −79° C.;(B) up to 40 phr of polybutadiene having a cis 1,4 content greater than 95 percent and a Tg ranging from −80 to −110° C.;(C) from 30 to 80 phr of a combination of a resin having a Tg of at least 30° C. and an oil, wherein the weight ratio of resin to oil is greater than 1.