An additive manufactured product, along with methods of its formation, is provided. The additive manufactured product may include a fused multilayer component comprising a nickel superalloy having a composition comprising, by weight: 7% to 11% of cobalt; 9% to 14% of chromium; 1.5% to 8% of molybdenum; up to 8% of tungsten; 4% to 6% of aluminum; 1% to 4% of titanium; up to 4.6% tantalum; up to 2% hafnium; up to 0.04% zirconium; up to 0.05% carbon; up to 0.04% boron; up to 1% niobium; and the balance nickel along with unavoidable residual elements in trace amounts. This composition may have a sum of the weight percentages of zirconium and boron that is up to 0.06%.
Timeline
No Timeline data yet.
Further Resources
No Further Resources data yet.