Coating material (237) for generating a coating layer by non-impact printing wherein the coating layer represents an image and wherein a resolution of the image is at least 100 DPI, the coating material comprising a curable resin; wherein the coating material (237) exhibits a minimum viscosity when being heated from room temperature with a heating rate of 5 Kelvin per minute up to a temperature where curing of the coating material occurs, wherein the minimum viscosity is in a range between 3 Pascal seconds to 20000 Pascal seconds, in particular in a range between 50 Pascal seconds and 10000 Pascal seconds and further in particular in a range between 250 Pascal seconds and 7000 Pascal seconds; and wherein a pill flow length is below 350 mm at a potential curing temperature which may be used to cure the coating material.