Patent 11084756 was granted and assigned to Corning Incorporated on August, 2021 by the United States Patent and Trademark Office.
Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of compression DOC of at least about 125 μm within the glass article. The compressive stress profile includes a single linear segment or portion extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile may include an additional portion extending from the surface to a relatively shallow depth and the linear portion extending from the shallow depth to the depth of compression.