Patent attributes
The embodiments described herein relate to glass articles that include mechanically durable glass compositions having high liquidus viscosity. The glass articles may include glass compositions having from 50 mol. % to 80 mol. % SiO2; from 7 mol. % to 25 mol. % Al2O3; from 2 mol. % to about 14 mol. % Li2O; 0.4 mol. % P2O5; and less than or equal to 0.5 mol. % ZrO2. The quantity (Al2O3 (mol. %)−R2O (mol. %)−RO (mol. %)) is greater than zero, where R2O (mol. %) is the sum of the molar amounts of Li2O, Na2O, K2O, Rb2O, and Cs2O in the glass composition and RO (mol. %) is the sum of the molar amounts of BeO, MgO, CaO, SrO, BaO, and ZnO in the glass composition. A molar ratio of (Li2O (mol. %))/(R2O (mol. %)) may be greater or equal to 0.5. In embodiments, the glass composition may include B2O3. The glass compositions are fusion formable and have high damage resistance.