A sintered R-T-B based magnet includes a main phase crystal grain and a grain boundary phase, in which R: not less than 27.5 mass % and not more than 35.0 mass % (R always includes at least Nd and Pr); B: not less than 0.80 mass % and not more than 1.05 mass %; Ga: not less than 0.05 mass % and not more than 1.0 mass %; M: not more than 2 mass % (where M is at least one of Cu, Al, Nb, and Zr); and a balance T (where T is Fe, or Fe and Co) and impurities. At 300-μm depth from the magnet surface, a Pr/Nd ratio in a central portion of a main phase crystal grain is lower than 1, and a Pr/Nd ratio in an intergranular grain boundary is higher than 1. The Ga concentration gradually decreases in a portion of the magnet from the surface toward the interior.