Patent attributes
A manufacturing method of ceramic powder includes: synthesizing barium titanate powder from barium carbonate, titanium dioxide, manganese carbonate, and one of ammonium molybdate and tungsten oxide, wherein: a solid solution amount of the donor element is 0.05 mol or more and 0.3 mol or less; a solid solution amount of the accepter element with respect to the barium titanate is 0.02 mol or more and 0.2 mol or less on a presumption that the amount of the barium titanate is 100 mol and the acceptor element is converted into an oxide; and relationships y≥−0.0003x+1.0106, y≤−0.0002x+1.0114, 4≤x≤25 and y≤1.0099 are satisfied when a specific surface area of the ceramic powder is “x” and an axial ratio c/a of the ceramic powder is “y”.