Patent attributes
A thin film formation method includes setting a film formation subject to 200° C. or higher. A first step includes changing a first state, in which a film formation material and a carrier gas are supplied so that the film formation material collects on the film formation subject, to a second state, in which the film formation material is omitted. A second step includes changing a third state, in which a hydrogen gas and a carrier gas are supplied to reduce the film formation material, to a fourth state, in which the hydrogen gas is omitted. The film formation material is any one of Al(CxH2x+1)3, Al(CxH2x+1)2H, and Al(CxH2x+1)2Cl. The first step and the second step are alternately repeated to form an aluminum carbide film on the film formation subject such that a content rate of aluminum atoms is 20 atomic percent or greater.