The present invention relates to a cable jacket comprising a random heterophasic propylene copolymer, wherein said copolymer comprises a matrix (M) being a random propylene copolymer (R-PP) and dispersed therein an elastomeric propylene copolymer (E), wherein the random propylene copolymer (R-PP) has a melt flow rate MFR2 (230° C./2.16 kg) of 0.1 to 10.0 g/10 min and wherein the elastomeric propylene copolymer (E) has a comonomer content in the range of 40.0 to 55.0 mol %, and wherein said copolymer has MFR2 (230° C.) in the range of from 0.5 to 15 g/10 min, flexural modulus below 400 MPa, and relaxation spectrum index (RSI) at 200° C. below 20.0. The present invention further relates to a telecommunication cable comprising said jacket.