Patent attributes
A thermoplastic polymer composition comprises a polyethylene polymer composition and a salt of bicyclo[2.2.1]heptane-2,3-dicarboxylic acid. The polyethylene polymer composition can have a Melt Relaxation Ratio of 1.5 or greater. A method for molding a thermoplastic polymer composition comprises the steps of (a) providing an apparatus comprising a die and a mold cavity; (b) providing the thermoplastic polymer composition described above; (c) heating the thermoplastic polymer composition to melt the thermoplastic polymer composition; (d) extruding the molten thermoplastic polymer composition through the die to form a parison; (e) capturing the parison in the mold cavity; (f) blowing a pressurized fluid into the parison to inflate the parison and conform it to the interior surface of the mold cavity; (g) allowing the molded article to cool so that the molded article retains its shape; and (h) removing the molded article from the mold cavity.