A method of manufacturing a waterproof strapped accessory and a waterproof strapped accessory formed according to the disclosed method are provided. Using a thermal laser cutter, a raw thermal polyurethane-coated nylon webbing material is cut, obtaining a desired shape of a strapped accessory. Holes may be cut through the strapped accessory using the thermal laser cutter. The thermal laser cutter seals the cut edges of the strapped accessory as well as any hole cut by the thermal laser cutter, rendering all or most edges waterproof. The strapped accessory is then inspected, and any unsealed edges sealed with a thermal rod. The strapped accessory is then cleaned of any residue and allow to cure under predetermined environmental conditions for a predetermined amount of time. Keepers and/or any desired hardware may be affixed to the strapped accessory. Indicia may also be imparted onto the strapped accessory by the thermal laser cutter.