Patent 12103267 was granted and assigned to Pratt & Whitney Canada on October, 2024 by the United States Patent and Trademark Office.
A coating-substrate combination includes: a Ni-based superalloy substrate comprising, by weight percent: 2.0-5.1 Cr; 0.9-3.3 Mo; 3.9-9.8 W; 2.2-6.8 Ta; 5.4-6.5 Al; 1.8-12.8 Co; 2.8-5.8 Re; 2.8-7.2 Ru; and a coating comprising, exclusive of Pt group elements, by weight percent: Ni as a largest content; 5.8-9.3 Al; 4.4-25 Cr; 3.0-13.5 Co; up to 6.0 Ta, if any; up to 6.2 W, if any; up to 2.4 Mo, if any; 0.3-0.6 Hf; 0.1-0.4 Si; up to 0.6 Y, if any; up to 0.4 Zr, if any; up to 1.0 Re, if any.