Patent abstract
In a method of producing a lithium niobate substrate by the use of a lithium niobate crystal grown by the Czochralski process, the lithium niobate crystal is heat-treated at a temperature of from 300° C. or more to less than 500° C. in the state the lithium niobate crystal is buried in a powder constituted of at least one element selected from the group consisting of Al, Ti, Si, Ca, Mg and C, or in the state the lithium niobate crystal is held in a container constituted of at least one element selected from the group consisting of Al, Ti, Si, Ca, Mg and C.