Patent attributes
A method for producing a tantalum PVD component includes a minimum of three stages, each of which include a deformation step followed by a high-temperature anneal. The deformation occurs in air and at a component temperature less than or equal to 750° F. in at least one of the minimum of three stages. The anneal occurs at a component temperature of at least 2200° F. in at least the first two of the minimum of three stages. The tantalum component exhibits a uniform texture that is predominately {111}<uvw>. As an alternative, the deformation may occur at a component temperature of from 200° F. to 750° F. in at least the last stage of the minimum of three stages. The anneal may occur at a component temperature of from 1500° F. to 2800° F. in at least three of the minimum of three stages.