Patent attributes
In the present invention, a coating liquid satisfies the liquid physical property conditions: (A) in the drying process, after the solid content concentration in the coating liquid is increased to 15% by mass or more by drying the coating film, or after the start of drying when the solid content concentration in the coating liquid is 15% by mass or more at the time of coating; (B) the shear viscosity of the coating liquid becomes 5 mPas or more for the shear rate of 103 sec−1 or less; (C) the value obtained through dividing by the average viscosity the first differential coefficient, the increase coefficient of the increase rate of the shear viscosity relative to the increase rate of the solid content concentration is 0.15 or more; and (D) the second differential coefficient, an additional increase coefficient of the increase coefficient relative to the solid content concentration is positive.