A process for brazing components formed of superalloys that contain elements prone to oxidation during brazing. At least one braze tape is applied to at least one faying surface of at least a first of the components being joined by brazing. The braze tape comprises a braze tape alloy containing the base metal of the superalloys and a melting point suppressant, and is applied so as to substantially cover the faying surface. The braze tape is then bonded to the faying surface by heating the first component to a temperature not exceeding the brazing temperature required to join the components. Thereafter, the components are assembled so that the bonded braze tape are between the respective faying surfaces of the components. The components are then brazed together by applying and heating a braze alloy to the braze temperature.