Patent attributes
Methods for the production of carbon foam from swelling coals that do not require the use of high process pressures, oxidized coal, devolatized coal, or high-strength, foam expansion confining molds are described. In some embodiments, a comminuted swelling bituminous coal is heated to a first elevated temperature sufficient to result in the coal particles softening and melting together to form a substantially homogeneous open cell plastic carbon material. The substantially homogeneous open cell plastic carbon material may then be heated to a second elevated temperature at a slow rate to form carbon foam. In some embodiments, the resulting carbon foam may be heated to a higher third elevated temperature. The resulting carbon foam may be subsequently heated to elevated temperatures as great as 3200° C. or more.