Patent attributes
The aggregated particles are manufactured through a method of manufacturing aggregated particles, which includes an aggregating step, a depressurizing step, and a cooling step. In the aggregating step, a slurry is prepared which contains aggregated particles obtained by flowing an aqueous slurry of resin fine particles having a volume average particle diameter in the range of 0.4 μm to 3 μm through a coiled piping in a heated and pressurized state and thereby aggregating the resin fine particles. In the depressurizing step, the slurry containing the aggregated particles is depressurized, and a particle size control is conducted by disintegrating coarse particles so as to homogenize particle diameters of the aggregated particles. In the cooling step, the slurry containing the aggregated particles of which particle diameters have been homogenized is cooled.