A process comprises polymerizing an olefin monomer in a loop reactor in the presence of a catalyst and a diluent, and producing a slurry comprising solid particulate olefin polymer and diluent. The Biot number is maintained at or below about 3.0 within the loop reactor during the polymerizing process. The slurry in the loop reactor forms a slurry film having a film coefficient along an inner surface of the reactor wall, and the film coefficient is less than about 500 BTU·hr−1·ft−2·° F.−1.