Patent attributes
Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and an equibiaxial flexural strength of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.