Patent attributes
A hexagonal single crystal wafer is produced from a hexagonal single crystal ingot. A separation start point is formed by setting a focal point of a laser beam inside the ingot at a predetermined depth from the upper surface of the ingot, which depth corresponds to a thickness of the wafer to be produced. The laser beam is applied to the upper surface of the ingot while relatively moving the focal point and the ingot to thereby form a modified layer parallel to the upper surface of the ingot and form cracks extending from the modified layer along a c-plane, thus forming a separation start point. The wafer is separated by immersing the ingot in water and then applying ultrasonic vibration to the ingot, thereby separating a plate-shaped member having a thickness corresponding to the thickness of the wafer from the ingot.