An average value of a hydrogen content ratio of a surface layer made of hydrogenated amorphous carbon is set to be 0.40 or less and a maximum value of an sp2 bonding ratio in an outermost surface region of the surface layer made of the hydrogenated amorphous carbon is set to be 0.50 or less.