In an embodiment, a method includes: bonding a back side of a first memory device to a front side of a second memory device with dielectric-to-dielectric bonds and with metal-to-metal bonds; after the bonding, forming first conductive bumps through a first dielectric layer at a front side of the first memory device, the first conductive bumps raised from a major surface of the first dielectric layer; testing the first memory device and the second memory device using the first conductive bumps; and after the testing, attaching a logic device to the first conductive bumps with reflowable connectors.